Abstract
In an earlier communication ESR measurements on de-oxygenized selenium were announced. The present paper reports on further ESR measurements on liquid de-oxygenized selenium carried out in a temperature interval 240}o{C < T < 420}o{C. The g-value of the ESR signal is found to be 2.03 +/- 0.02. The temperature dependence
... read more