Abstract
Ni contamination from crude oil in the fluid catalytic cracking (FCC) process is one of the primary sources of catalyst deactivation, thereby promoting dehydrogenation–hydrogenation and speeding up coke growth. Herein, single-particle X-ray fluorescence, diffraction and absorption (μXRF-μXRD-μXAS) tomography is used in combination with confocal fluorescence microscopy (CFM) after thiophene staining