Silicon oxynitride films with five different O/N ratios were deposited with low pressure chemical vapor deposition on a silicon substrate covered with an oxide. The films were subjected to subsequent post-deposition anneals in N2 and H2 at 1000°C, and a H plasma at 300°C to obtain information about the hydrogen